In the world of mining excavation, basalt is nicknamed “hard bone” by many construction bosses due to its high consumption of cutting tools. In fact, this is a misunderstanding of it. Compared with granite and quartzite, basalt can be regarded as a “gentle” stratum.
Today, Merinmate combines years of field experience in dismantling basalt working conditions to help you identify the weak points of basalt and accurately break the rock, making your picks truly durable and greatly improving construction efficiency.
Why is “gentle” basalt so difficult to work with?
As the saying goes, only by knowing yourself and the enemy can you be invincible in every battle. If you want to “get basalt”, you must first understand its three characteristics:

1. High density results in no “breakthrough” to exploit
Basalt has few pores, a dense structure, and a volume density of up to 2.8-3.0g/cm³. This means that there are almost no “weak points” inside the rock. The picks need to destroy it purely by cutting, rather than using cracks to expand. Therefore, even if the hardness of the basalt is not high, continued friction and extrusion will quickly wear out the picks.
2. Extremely abrasive, comparable to “sandpaper”
It is rich in hard minerals such as pyroxene and plagioclase. These minerals have small particles and high hardness. They are like countless micro files. When the pick and the rock rub at high speed, it will cause severe wear and tear on the cutter head. At the same time, the friction generates high temperatures, which further aggravates the failure of the pick. This is the core reason for tooth wear.
3. Both brittle and tough – the impact is “caught off guard”
The toughness of basalt is between that of granite and limestone. When cutting, it will not simply collapse like highly brittle rocks, but will show “viscous failure” – it will not collapse when cut in, nor will it be removed when ground, and the pick will drag in the rock for a longer time. This characteristic, coupled with local structural unevenness, can easily produce instantaneous high impact loads, leading to chipping and broken teeth. At the same time, high-frequency impacts can also aggravate the internal damage of the alloy.
Practical pain points: Under working conditions such as basalt, pick failure mainly occurs in four forms, each corresponding to a clear source of failure. Melinmate also provides exclusive selection techniques and construction method optimization for reference:

1. The alloy head cracks – “insufficient impact resistance”
Performance of picks: The tooth head loses pieces and chips, and the cutting ability is lost instantly.
Reason: If the pick is made of an ordinary alloy grade, or the grain size is not fine enough, it will break like glass under a huge impact.
2. The alloy head is quickly ground flat – “the “red hardness” cannot bear it”
Performance: The tooth tips become shorter, energy consumption increases, and the excavation speed slows down.
Reason: High-speed friction between the pick and the rock produces high temperature. If the hardness of the alloy (the ability to maintain hardness at high temperatures) is insufficient, the tooth tips will be quickly rounded and become “bald”, resulting in a significant decrease in excavation efficiency.
3. The alloy head falls off – the “weld seam” cannot withstand the high temperature.
Performance: The whole tooth falls off, which not only loses consumables, but may also damage the cutting arm of the tunnel boring machine.
Reason: The basalt working conditions continue to be high. If the brazing process is not in place (such as uneven weld gaps and residual stress), or the solder has poor heat resistance, the joint between the alloy head and the tooth body will soften and crack, eventually leading to a “U-turn.”

4. Appearance is intact but fails – “high temperature internal injury”
Performance: The tooth head is intact and not bald, and the excavation efficiency is getting lower and lower. It seems that it is not broken, but in fact it has failed.
Reason: long-term cutting in basalt formations, friction generates continuous high temperatures, resulting in a decrease in the hardness of the alloy red. The surface looks intact, but the internal hardness has been greatly attenuated, forming an invisible scrap of “no obvious wear, but failure”.
Strategy to break the situation: The selection strategy does not copy granite. In view of the “abrasion-dominated” characteristics of basalt, the selection ideas need to be adjusted:
1. Tooth wear resistance is the first priority:
Preferred choice in basalt working conditions:
- The front part of the tooth body is surfacing with high temperature and wear-resistant coating (thickness 2-3mm)
- Use wear-resistant materials such as high chromium cast iron to strengthen the teeth
- Uniform transition of tooth hardness to avoid local “soft spots”
2. Alloy head: toughness takes precedence over ultra-high hardness
Use ultra-fine grain alloy. Its grains are finer and the structure is denser, which can effectively disperse the impact load, greatly improve the resistance to cracking, and perfectly cope with the instantaneous high impact during basalt cutting.

3. Weld strength: prevent “the tooth body is still there without the head”
When the tooth body is worn to a certain extent, the weld will be exposed. If the weld itself is not strong enough, the alloy head will fall off completely even if it is not completely worn out. Melinmate uses a vacuum brazing process. Even if the tooth body is worn to the limit, the weld can still “hold up”.
4. Pick shape: Priority is given to tapered teeth.
The tapered teeth have good self-rotation performance and can effectively resist eccentric wear, making them more suitable for highly abrasive basalt.
5. Construction method optimization
Mailinmat reminds: During the construction process, skill is more important than brute force, and construction methods should be adjusted appropriately.
- Control the feed: Appropriately reduce the cutting speed, increase the cutting depth, avoid high-frequency friction of the picks at the same position, and reduce heat generation. This can not only alleviate the decrease in alloy red hardness, but also reduce tooth body wear and brazing layer softening.
- Timely inspection: Under basalt working conditions, tooth chipping and invisible failure are normal. In addition to checking the appearance of the pick for wear and chipping, we should also pay attention to changes in excavation efficiency. Once it is found that the rock breaking is ineffective, replace it in time to avoid ineffective consumption and tooth seat damage.
Final summary

Basalt is not the hardest rock, but it is one of the most “grindable” rocks. Choosing the right pick is half the battle; using the right construction method is the icing on the cake.
Mailinmat has been deeply involved in tunneling tools for many years and has accumulated rich practical experience in different working conditions such as basalt and granite. If you also encounter the problem of “not hard but tooth-weary” during construction, please leave a message to communicate, and we will discuss ways to break the rock together.