In coal mining and tunnel boring, the service life of picks directly governs project costs and progress.
Yet the primary bottleneck often lies neither in the ultra-hard carbide tip, nor the tough steel pick body — it is the thin brazing layer sandwiched between them. This is the “throat” of the pick.
01 What is the brazing layer? Like tooth root and concrete
A pick consists of two parts:
- Front end: High-hardness cemented carbide tip (typically tungsten-cobalt alloy), which cuts and breaks rock.
- Rear shank: High-toughness steel body, which absorbs impact loads.
One is built for hard rock cutting, the other for shock resistance. Each has its own strengths.
Here comes the question: how to firmly join these two dissimilar materials into one integrated component? The answer is brazing.
The brazing layer is the bonding layer formed between the carbide tip and steel shank via the brazing process. It acts like concrete in a structure, locking the “brick” (carbide tip) to the “reinforcement bar” (steel body).
To put it simply: The carbide tip = the pick’s “crown of the tooth” The steel shank = the pick’s “jawbone” The brazing layer = the pick’s “tooth root” — invisible, yet it determines whether the whole pick stays firmly anchored under relentless impact.

02 Why does the brazing layer matter so much? The main culprit for tip loss
Many operators have encountered this issue: Shortly after picks go underground, the carbide tip falls off. Both tip and shank remain intact, yet they separate. The entire pick becomes scrap.
Carbide tip shedding is one of the dominant failure modes for mining conical picks, and poor brazing quality of the brazing layer is the leading cause.
Think about the loads picks endure underground:
⚡ Extreme impact loads
🔄 Complex alternating stress
🌡️ Severe temperature fluctuations
All these forces converge on this brazed joint.

- A high-quality brazing layer: effectively prevents tip shedding and pick fracture
- A defective brazing layer: no matter how hard the carbide or how good the steel, premature failure is inevitable
In short: brazing layer quality directly decides pick service life and operational safety.
03 Why does the brazing layer fail easily? Five interlinked weak points
Thin as it is, the brazing layer involves multiple critical variables. Any misstep undermines its performance:
| Influencing factor | Consequence |
|---|---|
| Improper brazing filler metal | Great differences in wettability and mechanical properties; wrong filler leads to joint failure |
| Uncontrolled brazing gap | Steel and carbide have different thermal expansion coefficients. Too wide = insufficient filler penetration; too narrow = restricted filler flow |
| Inappropriate brazing temperature | Excessive heat damages carbide; insufficient heat prevents full melting of brazing alloy |
| Inadequate pre-cleaning | Residual oxide and grease cause poor bonding, resulting in cold solder joints |
| Excessive residual stress | Mismatched thermal expansion creates heavy stress during cooling, which may crack the joint |
These factors are closely connected. Failure at any step turns the brazing layer into the weakest link of the pick.

04 Our solution: Treat brazing quality as our lifeline
As a pick manufacturer, we understand: What our customers need is not merely a pick, but reliable performance that stands up to harsh underground conditions.
We have adopted advanced vacuum brazing technology:
✅ Brazing takes place in a vacuum environment, fully isolated from oxygen
✅ Eliminates oxidation and slag inclusions inside the joint
✅ Greatly improves bonding strength and fatigue resistance of the brazing layer
From brazing material selection and gap control, to precise temperature regulation inside vacuum furnaces, every detail is strictly controlled.

💬 Closing notes Feel free to leave a comment or message us for more technical details and quality standards of pick brazing layers.
We do not just manufacture picks. We safeguard every metre of your underground advance.